Abstract

Wire bonding plays a critical role in the MEMS pressure sensor packaging process. The performance of wire bonding directly determines the functionality and service life of pressure sensors. During reliability qualification of safe-launch sample builds, wire-bond bump-ball lift was observed on the ASIC die of a stacked-die pressure sensor after 1000 cycles of temperature cycling. However, there are numerous factors affecting wire bond performance, including wire bond parameters, bond pad contamination, plasma cleaning effectiveness and process variation. Accordingly, this study investigated the root cause of this issue. The DOE results indicated that silicon glue staging time is a key factor affecting pad contamination. This contamination impaired the interfacial integrity between the bump ball and bond pad, as reflected in low ball shear strength, and ultimately led to ball lift after temperature cycling testing. Ball shear strength tests with staging time DOE units showed that from a staging time of 3 hours to 12 hours, the average ball shear strength decreased from 31.30 g to 27.22 g. Optimizing wire bond parameters can significantly improve ball shear strength and reduce the effect of pad contamination associated with silicon glue staging time. With the improved wire-bond parameters, the average ball shear strength was 31.06 g after 12 hours of staging. Furthermore, improvement actions for products with similar structures are proposed and discussed based on the experimental results.

Keywords: Stacked Die; Wire Bonding; Ball Shear; Silicon Glue Staging Time; Wire Bonding Parameters
Published: October 20, 2026
DOI: 10.54254/2755-2721/2026.37765
Volume: ACE Vol.277
pp. 42-49
Download PDF

References

  1. Vath, J. C., Srikanth, N., & Murali, S. (2004). An evaluation of gold and copper wire bonds on shear and pull testing.Journal of Electronic Packaging, 128(3), 192–201. DOI: 10.1115/1.2229214.
  2. Yen, L. H., & Lai, I. F. (2025). Solving bump bonding issues with 2.0 mil copper wire: A study on FSM integration and workability improvements.Microelectronics Reliability, 167, 115628–115628. DOI: 10.1016/J.MICROREL.2025.115628.
  3. Knotter, M. D., Rink, A. I., Claassen, A. W., et al. (2011). Bond pad surface quality for reliable wire bonding.Microelectronic Engineering, 88(12), 3452–3458. DOI: 10.1016/j.mee.2011.01.075.
  4. M., K., T., T., & H., F. (1987). Aluminum bond pad contamination by thermal outgassing of organic material from silver-filled epoxy adhesives.IEEE Transactions on Components, Hybrids, and Manufacturing Technology, 10(4), 586–592. DOI: 10.1109/tchmt.1987.1134781.
  5. Maleki, P., Safar, A. A., Marques, A. E., et al. (2026). Failure analysis of interconnections and bi-material interfaces in microelectronic packages and semiconductors: A review.Engineering Failure Analysis, 197(PB), 111242–111242. DOI: 10.1016/J.ENGFAILANAL.2026.111242.
  6. He, L., & Liu, H. T. (2017). Failure mechanisms and analysis of wire bonding.Microprocessors, 38(6), 17–20. (in Chinese)
  7. Patents; researchers submit patent application, "Wire bond cleaning method and wire bonding recovery process", for approval (USPTO 20170110437).Chemicals & Chemistry, 5910.
  8. Li, X., Du, Y. H., Gao, L. Y., et al. (2024). Effect of plasma cleaning on the surface condition and mechanical properties of Cu/Al wire-bonded joints.Transactions of the China Welding Institution, 45(12), 14–19. (in Chinese)
  9. Kung, T. A., Bang, S. H., & Bang, S. H. (2006). Irregular characteristics of bond interface formation in ultrasonic wire wedge bonding.Journal of Materials Science & Technology(4), 483–486.
  10. Gan, L. C., Classe, et al. (2014). Effects of bonding wires and epoxy molding compound on gold and copper ball bonds intermetallic growth kinetics in electronic packaging.Journal of Electronic Materials, 43(4), 1017–1025. DOI: 10.1007/s11664-014-3011-y.
  11. Olander, B., Wirsén, A., & Albertsson, A. (2003). Silicone elastomers with controlled surface composition using argon or hydrogen plasma treatment.Journal of Applied Polymer Science, 90(5), 1378–1383. DOI: 10.1002/app.12835.
  12. Hino, T., Igarashi, Y., Ymauchi, Y., et al. (2008). Surface wettability of silicon rubber after irradiation with a glow discharge plasma.Vacuum, 83(3), 506–509. DOI: 10.1016/j.vacuum.2008.04.015.